Attention Contractors! Here's what to know about Field Testing Concrete

The plans have been approved, the foundation has been poured....But hold up! There is a delay in construction due to a fault in concrete field testing.... The dreaded words that no contractor wants to hear.


Did you know that to test concrete in Georgia, concrete field technicians must be certified by

ACI? This change came to Georgia Building Code in 2018. Since this change the GRMCA hopes that concrete testing has improved as more qualified field technicians enter the workforce. To verify a certification you can visit concrete.org/verfiy


Here are several important areas of field testing for contractors to understand and track


From ForConstructionPros.Com


Slump Measurement

It may seem odd, but field testing the compressive strength of concrete starts long before it sets or cures on the jobsite. Measuring the consistency of the concrete, or slump following ASTM C 143 to confirm it’s within the specified range is the first step in field testing.

While ready mix concrete producers simply report the slump prior to delivery, for packaged concrete manufacturers, it’s important that the quantity of water added in the field is both documented and confirmed to produce a slump within the manufacturer’s specified range for that concrete. A standard pre-packaged concrete typically specifies a slump of 2 to 3 inches, while there are other concretes designed to be used at a higher slump, such as 3 to 5 inches to meet or exceed specific project requirements. The more water that is added to a given concrete, the higher the slump it will have. The higher the slump for a given concrete, the lower the strengths, so it is critical to stay within the specified slump range.


Curing Conditions

Understanding the jobsite enviornment also plays an important role in field testing the compressive strength of concrete specimens. If a concrete specimen freezes within the first 24 hours after being molded, or before it has reached a minimum strength of approximately 500 PSI, it will lose significant overall strength. Because of this, concrete specimens should be stored for up to 48 hours in a moist environment having a temperature of 60 °F to 80 °F (16 °C to 27 °C).


In addition, concrete specimens should not be exposed to direct sunlight or radiant heating, as these conditions would cause the concrete specimens to lose some of the water needed to react with the cement for strength gain.


After completion of initial curing, but within 30 minutes of specimens being demolded, the environment in which the specimens are stored must be even more tightly controlled, with a temperature of 70 °F to 77 °F (21 °C to 25 °C). There must be free water on the specimens at all times, which can be achieved through use of water storage tanks or moist rooms. By closely managing these conditions during the entire remaining curing process, the field created samples should accurately reflect the compressive strength of the concrete.


Specimen Preparation

It may be surprising how many factors can impact the quality of the cylindrical concrete specimens, which ultimately are used to determine the compressive strength. Poorly made specimens may produce false low compressive strength results. The number of concrete cylinders to be cast for each test age is typically dictated by the project requirements. If the number is not specified, no fewer than two, and preferably three, are generally recommended for each test age. A single specimen will not provide sufficient data to indicate if that specimen was faulty.


The specimens must be cast on a flat and level surface that is not exposed to any movement due to nearby forklift, crane or other vehicular traffic, or even nearby concrete mixers in operation.


The method used to place the concrete into the cylindrical molds (of size as directed by project requirements) is also critical. The concrete must be added in multiple layers, with the exact number of layers depending upon the size of the aggregate. Each layer must be of approximately equal depth and consolidated, typically by rodding and tapping the outside of the mold. Not following the consolidation requirements as defined in ASTM C 31 can leave air voids, which will produce false low compressive strength results. Similar to finishing a slab, the concrete at the surface of the cylindrical molds should not be overworked. The finished surface should be a flat and even with no pits or bumps greater than 1/8 inch. If not, it will result in uneven contact with the platens of the compressive strength machine, which again, may result in false low compressive strength results.


Transportation

As we all know, damage can occur during the transportation of anything from one place to another. Concrete specimens are no different. Specimens should never be transported until at least 8 hours after the concrete has achieved final set. Final set is when the concrete has completely lost its plasticity and has hardened. If the concrete specimens are moved sooner than eight hours after final set, they may be damaged, causing false low compressive strength results.


During transportation, moisture loss must be prevented by covering with plastic or wet burlap like that used when curing concrete slabs or by using other means. Loss of moisture will result in lower compressive strength results of the specimens.


Break Testing

With proper slump, curing conditions, specimen preparation and transportation verified, the final and ultimate test begins. Each secured concrete cylinder should undergo a break test at the manufacturer’s laboratory or other approved third-party facility. The equipment should always be properly calibrated. The load should be maintained at a rate of 27 to 42 psi/second. Testing should be continued until the sample fails and presents a well-defined fracture.


The strength of the concrete is determined by dividing the maximum load by the area of the cylinder’s end. Calculate the average of all specimens from the same test age then round to the nearest 10 psi. If measured strength is lower than expected, examine the specimens to see if they are manifestly faulty, for example, if they contain large air voids indicating that they were not properly compacted. Results of any such specimens should be discarded.

When the standard procedures for field testing are followed correctly, contractors can count on concrete that will keep projects on schedule.